Bayer poisons: degradation of klason lignin in sodium hydroxide at 145°C

Amanda Ellis, Michael Wilson, Peter Forster

    Research output: Contribution to journalArticlepeer-review

    16 Citations (Scopus)
    Original languageEnglish
    Pages (from-to)6493-6502
    Number of pages10
    JournalIndustrial and Engineering Chemistry Research
    Volume41
    Issue number25
    Publication statusPublished - 2002

    Cite this